1,2,3,6-Tetrahydrophthalic anhydride (THPA, CAS 85-43-8) is the Diels-Alder adduct of butadiene and maleic anhydride: a white flake with a melting point near 100 deg C, one anhydride group and one isolated ring double bond. It is used as an epoxy curing agent for electrical castings, as a resin and polyester intermediate, and as a building block where the retained double bond is wanted for later crosslinking.
Basic Information
| CAS Number | 85-43-8 |
| Synonyms | THPA; 1,2,3,6-tetrahydrophthalic anhydride; 4-cyclohexene-1,2-dicarboxylic anhydride; tetrahydrophthalic anhydride |
| Molecular Formula | C8H8O3 |
| Molecular Weight | 152.15 g/mol |
| Anhydride groups per molecule | 1 |
| Anhydride equivalent weight | 152.15 g/eq (theoretical) |
| PubChem CID | 6810 |
| InChIKey | KMOUUZVZFBCRAM-UHFFFAOYSA-N |
| SMILES | C1C=CCC2C1C(=O)OC2=O |
| IUPAC name | 3a,4,7,7a-tetrahydro-2-benzofuran-1,3-dione |
| Appearance | White flake or fused solid |
| Melting point | About 100 deg C (specified 100 +/- 2 deg C) |
| Chemical family | Cycloaliphatic dicarboxylic anhydride |
Specifications
Four grades are offered. The two standard grades differ in colour and assay; the two custom grades add free-acid, ash, iron and a customer-specific anti-shrinkage requirement for customers running electrical or optical castings.
| Item | Grade 1 (standard) | Grade 2 (custom) | Grade 3 (standard) | Grade 4 (custom) |
|---|---|---|---|---|
| Appearance | White flake | White flake | White flake | White flake |
| Assay (anhydride content) | >=99.0% | >=99.0% | >=99.5% | >=99.5% |
| Colour, Hazen/APHA (as quoted) | <=80 | <=30 or <=50 | <=60 | <=30 |
| Melting point | 100 +/- 2 deg C | – | 100 +/- 2 deg C | – |
| Free acid | – | <=0.2% or <=0.5% | – | <=0.2% or <=0.5% |
| Ash | – | <=0.005% | – | <=0.005% |
| Iron | – | <=10 ppm | – | <=10 ppm |
| Silicon-free anti-shrinkage test | – | Compliant | – | Compliant |
What Separates the Four Grades
Assay and colour are the two axes. The 99.0% grades are the workhorses for general casting and resin work. The 99.5% grades exist because the residual 0.5% in a 99.0% lot is largely tetrahydrophthalic acid and low-boiling oligomers, and in a thick casting that residue changes both the cured colour and the cure schedule.
Free acid is a moisture history record, not a raw-material number. Every anhydride group that has hydrolysed is one group that will not react with epoxy. Running the arithmetic on a 0.2% free-acid limit shows why the custom grades are specified so tightly: one kilogram of water absorbed per tonne of flake hydrolyses about 8.4 kg of anhydride and forms about 9.4 kg of the diacid, which is a free-acid figure near 0.94%. In other words, 0.2% free acid corresponds to roughly 0.2 kg of water picked up per tonne, and the material has to be bagged and handled accordingly.
Iron below 10 ppm is a colour specification in disguise. Iron is the metal that most often gives a casting its yellow-brown tint, and it is also the ion that matters in electrical insulation. Ash below 0.005% works the same way: it is the inorganic residue that stays behind from catalyst, rust and packaging, and it is measured in parts per hundred thousand rather than percent for a reason.
The silicon-free anti-shrinkage test is a customer requirement, not a standard test. It is a compliance statement agreed with specific customers whose process is sensitive to silicone contamination and to shrinkage during cure. We supply it as declared, and we recommend that any new customer confirm the exact test method with us before writing it into a purchase specification.
Applications
- Epoxy curing agent for electrical castings. Dry-type transformers, instrument transformers, bushings, insulators and GIS components. Anhydride curing gives low exotherm, low shrinkage, high glass transition temperature and good electrical properties, which is why it dominates thick-section electrical casting rather than amine curing.
- Resin intermediate. Raw material for unsaturated polyester and alkyd resins, where the retained double bond allows later copolymerisation or crosslinking with styrene or acrylate monomers.
- Ester and plasticiser intermediate. Diester derivatives are used as plasticisers and as synthetic lubricant components.
- Diels-Alder building block. The same double bond that stays in the molecule makes THPA a convenient dienophile or diene partner for further cycloaddition chemistry, and a starting point for substituted cycloaliphatic diacids and diols.
- General purpose epoxy hardener for laminates, tooling and coatings where a solid, high-melting anhydride is convenient for pre-blended one-pack systems.
Formulating With THPA
Anhydrides react with epoxy resins through the anhydride ring, so the dose is set by equivalents rather than by weight alone:
phr = (AEW / EEW) x 100 x r
where AEW is the anhydride equivalent weight (152.15 for THPA), EEW is the epoxy equivalent weight of the resin, and r is the anhydride-to-epoxy molar ratio, normally 0.85 to 1.0 because the hydroxyl groups generated during cure consume part of the anhydride.
| Resin EEW | r = 0.85 | r = 0.90 | r = 1.00 |
|---|---|---|---|
| 185 (standard DGEBA) | 69.9 phr | 74.0 phr | 82.2 phr |
| 200 | 64.7 phr | 68.5 phr | 76.1 phr |
| 250 | 51.7 phr | 54.8 phr | 60.9 phr |
Anhydride cure is slow on its own and is normally accelerated. Typical accelerators are tertiary amines such as benzyldimethylamine, substituted imidazoles, and quaternary ammonium salts; cure temperatures for casting systems usually sit between 120 and 160 deg C with a post-cure step to develop the final glass transition. Because the reaction is not strongly exothermic, thick sections can be cured without the runaway that a fast amine system would create.
Handling and Storage
THPA melts at about 100 deg C, so it is supplied as flake and is either dosed as flake into a hot resin or melted in a dedicated heated vessel. Two practical rules follow. First, never heat it above the minimum needed: prolonged hot holding darkens the product and drives free acid upward. Second, keep melt lines and vessels dry, because water in a hot melt hydrolyses the anhydride immediately.
The solid is moisture sensitive and corrosive after hydrolysis. Store sealed, dry and away from amines, alkalis, alcohols and water. Handle with local exhaust ventilation, gloves, eye protection and a dust mask; the dust is irritating and the material is a skin sensitiser. Anhydride powder spills should be cleaned dry and never washed down with water, which turns the spill into a corrosive acid solution.
Do not store THPA in the same area as amine curing agents or accelerators. The two react exothermically on contact, and a leaking bag next to a leaking drum is a real incident scenario rather than a theoretical one.
Packaging and Supply
Standard packing is 25 kg net in paper sacks with a polyethylene inner liner, on shrink-wrapped pallets. For larger volumes we supply 500 kg or 1,000 kg jumbo bags with a moisture barrier liner, and we can quote lined steel drums or molten material in heated containers for customers with melt-handling equipment. Each lot ships with a certificate of analysis covering assay, colour, melting point and, for the custom grades, free acid, ash and iron. A safety data sheet accompanies the first shipment of each grade.
Chemical Structure
C1C=CCC2C1C(=O)OC2=O
Related Products
- 3,4,5,6-Tetrahydrophthalic anhydride (TMMA), CAS 2426-02-0
- Hexahydrophthalic anhydride (HHPA), CAS 85-42-7
- Methyltetrahydrophthalic anhydride (MTHPA), CAS 11070-44-3 – the liquid member, seven grades from Pt-Co 50 to 10.
- Methylhexahydrophthalic anhydride (MHHPA) on request
- Anhydride accelerators, epoxy resins and formulated casting systems on request
FAQ
Is THPA the same as 3,4,5,6-THPA? No. They share the formula C8H8O3 and the molecular weight 152.15 but differ in where the ring double bond sits, and that difference moves the melting point from about 100 deg C to about 67 deg C. They have different InChIKeys and are not interchangeable in a formulation without re-checking the melt handling and the cure schedule.
Why does the specification include a melting point? Because melting point is the fastest check on isomer identity and on the amount of the low-melting isomer present. A THPA lot that melts well below 98 deg C contains 3,4,5,6-isomer or acid, and both change the curing behaviour.
What free acid level should I specify? For electrical casting and any application where colour and cure schedule matter, 0.2% or below. For general resin intermediate use, 0.5% is usually workable. Remember that the free acid will rise in storage if the bag is opened in humid air, so specify the packing as well as the number.
Can THPA cure epoxy at room temperature? Not practically. Anhydride cure needs heat, typically 120 deg C and above, with an accelerator to bring the gel time into a workable range. Room-temperature anhydride cure exists in the literature but is not a production route for structural or electrical parts.
How should molten THPA be handled? In a dry, temperature-controlled melt system with a nitrogen blanket if available, kept at the lowest workable temperature, and never left hot overnight. Hot holding is the main cause of colour drift and free-acid increase in customer tanks.
Contact PolyblueChem for a current certificate of analysis, a sample of any of the four grades, and a quotation for flake, jumbo bag or molten supply.