1,2,4,5-Cyclohexanetetracarboxylic Dianhydride (HPMDA), CAS: 2754-41-8

1,2,4,5-Cyclohexanetetracarboxylic dianhydride (HPMDA, CAS 2754-41-8) is the hydrogenated analogue of pyromellitic dianhydride: same two anhydride rings, same roughly 110 g/eq anhydride equivalent weight, but an alicyclic backbone instead of a benzene ring. That single structural change is why HPMDA appears where PMDA cannot be used – colourless polyimide films, low-dielectric layers for high-frequency circuits, and transparent coatings that must survive UV without yellowing.

Status: The specification below is the current production grade. Polymorph, particle size, and electronic-grade metal limits are quoted against the actual requirement – ask for a lot COA before qualification, because this dianhydride hydrolyses readily and packaging history matters as much as purity.

Basic Information

CAS Number 2754-41-8
Chemical name 1,2,4,5-Cyclohexanetetracarboxylic dianhydride; HPMDA; cyclohexane-1,2,4,5-tetracarboxylic dianhydride
Molecular Formula C10H8O6
Molecular Weight 224.17 g/mol
PubChem CID 14453667
InChIKey LJMPOXUWPWEILS-UHFFFAOYSA-N
Chemical Family Alicyclic tetracarboxylic dianhydride (polyimide monomer)
Anhydride groups per molecule 2
Anhydride equivalent weight (AEW) 112.09 g/eq

Specification

Item Requirement
Appearance White to off-white crystalline powder
Purity (assay) 99% min
Anhydride equivalent weight 112.09 g/eq (theoretical, 224.17 / 2)
Acid value (theoretical) 500.6 mg KOH/g (2 x 56.11 x 1000 / 224.17)
Package 25 kg net, double polyethylene liner, nitrogen blanketed

Two derived numbers are worth carrying into any specification discussion, because they are what a QC lab can actually measure on incoming material. The theoretical acid value is 500.6 mg KOH/g: a lower figure usually means the lot has already partly hydrolysed to the tetra-acid, which consumes alkali before the anhydride rings open. The anhydride equivalent weight of 112.09 sets every stoichiometry downstream – 8.92 anhydride equivalents per kilogram, more than twice the figure for a mono-anhydride of the same mass such as Nadic anhydride (6.09 eq/kg).

Why the alicyclic backbone matters

PMDA (CAS 89-32-7) and HPMDA differ by six hydrogen atoms and one saturated ring, and their equivalent weights are within 3% of each other – 109.06 for PMDA against 112.09 for HPMDA. If the only thing you needed were anhydride equivalents, the two would be interchangeable. They are not interchangeable, because the benzene ring in PMDA is a chromophore and a rigid, planar, aromatic unit:

  • Colour. Aromatic polyimides absorb in the visible after imidisation – the familiar amber-to-brown PI film. The alicyclic ring has no such absorption, so HPMDA-based films stay colourless to pale yellow. That is the whole reason colourless polyimide (CPI) chemistry exists.
  • Dielectric behaviour. Removing the aromatic conjugation lowers dielectric loss, which is what matters for high-frequency substrates and antenna layers.
  • Flexibility and CTE. The cyclohexane ring is not planar, so the chain packs less tightly and the film is less brittle – but with a higher coefficient of thermal expansion than the aromatic analogue. CPI formulation work usually trades some of that back with rigid co-monomers.
  • Solubility. Alicyclic dianhydrides and their polyamic acids dissolve more readily in polar aprotic solvents, which is what makes spin-coating and slot-die formulations practical.

HPMDA against the common dianhydrides

Dianhydride CAS Formula / MW AEW Backbone Where it wins
HPMDA 2754-41-8 C10H8O6 / 224.17 112.09 Alicyclic Colourless film, low dielectric loss, good solubility
PMDA 89-32-7 C10H2O6 / 218.12 109.06 Aromatic Highest rigidity and heat resistance, lowest cost, amber film
Nadic anhydride (NA) 826-62-0 C9H8O3 / 164.16 164.16 Bridged alicyclic, mono-anhydride Epoxy curing, high Tg, low melt viscosity
Methyl Nadic anhydride (MNA) 25134-21-8 C10H10O3 / 178.18 178.18 Bridged alicyclic, liquid Liquid anhydride hardener for electrical casting
Hydrogenated MNA (H-MNA) 39973-36-9 C10H12O3 / 180.20 180.20 Bridged alicyclic, fully saturated Non-yellowing saturated system, light-stable castings

Read the AEW column and the backbone column together: the two-line comparison that matters in a specification meeting is not HPMDA against PMDA (3% apart on equivalents, worlds apart on colour) but HPMDA against the bridged mono-anhydrides, where the equivalent weight is 60% higher and the chemistry is a completely different application – epoxy curing rather than polyimide synthesis.

Hydrolysis: the number that decides whether your lot is good

Every anhydride ring opens with one molecule of water to give a diacid. HPMDA has two rings, so one mole (224.17 g) consumes two moles of water – 36.03 g. Inverted, that is the figure to keep on the bench:

  • 1 g of water deactivates 6.22 g of HPMDA. A solvent at 1,000 ppm water therefore destroys about 0.31% of the dianhydride solids in a 20% polyamic-acid solution; at 5,000 ppm it is past 1.5% and the molecular weight distribution starts to shift noticeably.
  • Store sealed under dry nitrogen, keep drums closed, and let cold drums come to room temperature before opening so that condensation does not form on the powder.
  • The first sign of hydrolysis in a reaction is not a failed batch but a viscosity that stops climbing, because one opened ring caps the chain end.

This is also why the acid value is the incoming test worth asking for. It catches hydrolysis before a film does.

Where it is used

Application What HPMDA contributes Typical partner
Colourless / transparent polyimide film and coatings (CPI) Alicyclic backbone with no visible absorption after imidisation Aromatic or alicyclic diamines; rigid co-monomers to control CTE
High-frequency laminates and dielectric layers Low dielectric loss, good planarising behaviour Fluorinated or alicyclic diamines
Photosensitive polyimide precursors Solubility of the polyamic acid, clean imidisation Photosensitive side groups on the diamine
Epoxy curing (secondary use) Very high crosslink density: 54.5 phr at EEW 185, r = 0.9 Liquid epoxy resins, accelerator at elevated temperature
Polyester and alkyd modification Two anhydride rings give a fast, high-functionality half-ester Polyols, at 150 to 200 degC

When HPMDA is used as an epoxy hardener rather than as a polyimide monomer, the dose arithmetic follows the usual rule: phr = AEW / EEW x 100 x r. At EEW 185 and a 0.9 stoichiometric ratio that is 54.5 phr – about 25% less material than Nadic anhydride in the same resin, because the molecule carries two anhydride groups. The price of that efficiency is brittleness: four ester linkages per molecule make a tightly crosslinked, high-Tg, low-elongation network, which is why it is normally blended with a flexible anhydride rather than used alone.

Handling and storage

Store in a cool, dry, well ventilated area, away from moisture and amines. Keep containers closed and under nitrogen where the process allows. Wear dust protection when handling powder; fine dianhydride dust is irritating to the respiratory tract. Dissolve into dry solvent rather than adding solvent to the powder, and keep the solution covered – polyamic acid solutions hydrolyse and lose molecular weight on standing.

Packaging and supply

Pack Typical user Note
25 kg net fibre drum, double PE liner, nitrogen blanket Pilot and production PI lines Standard export pack for moisture-sensitive dianhydrides
1 kg / 5 kg sample pack under nitrogen Formulation and qualification trials Ship with desiccant; use within weeks of opening
500 kg FIBC on request Continuous film lines Liner grade confirmed per order

Each lot ships with a COA covering assay and appearance at minimum; acid value, water content, and metal levels (for electronic grades) are reported on request. Export documents normally classify the product under HS 2917.20, the polycarboxylic acid anhydride heading. Tell us the solvent system and the target film colour at enquiry stage – a grade that performs in DMAc may need different handling in NMP.

FAQ

Is HPMDA a drop-in replacement for PMDA? On equivalents yes – 112.09 against 109.06 g/eq, under 3% apart, so the molar charge barely moves. On performance no: you trade heat resistance and cost for colour and dielectric loss. Reformulate the diamine side as well.

Why does the acid value matter if the assay is 99%? Assay by titration against the anhydride can still pass on a partly hydrolysed lot, because the tetra-acid also consumes alkali. A separate acid value, read against the theoretical 500.6 mg KOH/g, tells you whether the rings are intact.

Can it be used as an epoxy hardener? Yes, at 54.5 phr against EEW 185 at r = 0.9, but expect a brittle, high-Tg network. It is normally blended.

Contact PolyBlueChem for a lot COA, a nitrogen-purged sample and a quotation against your volume and destination port.

Related reading

Related Products

Scroll to Top