The Isomer With the Low Melting Point
3,4,5,6-Tetrahydrophthalic anhydride (CAS 2426-02-0) is one of two commercially available tetrahydrophthalic anhydrides, and it is the one that melts at about 67 deg C instead of about 100 deg C. The formula (C8H8O3), the molecular weight (152.15 g/mol) and the anhydride equivalent weight (152.15 g/eq) are identical to its better-known isomer; only the position of the ring double bond, and therefore a whole set of physical constants, is different.
The material is sold under a variety of names, and that is a procurement risk in itself. Some producers label it TMMA, some write 3,4,5,6-THPA, some use 1-cyclohexene-1,2-dicarboxylic anhydride, and the CAS number is sometimes printed without the isomer being named at all. This article sets out what the product is, what its three commercial grades are for, and what changes in the plant when you switch from the high-melting isomer to this one.
Chemical and Physical Properties
| Property | Value |
|---|---|
| CAS Registry Number | 2426-02-0 |
| IUPAC name | 4,5,6,7-tetrahydro-2-benzofuran-1,3-dione |
| Common synonyms | 3,4,5,6-Tetrahydrophthalic anhydride; TMMA (supplier designation); 1-cyclohexene-1,2-dicarboxylic anhydride |
| Molecular formula | C8H8O3 |
| Molecular weight | 152.15 g/mol |
| Anhydride equivalent weight | 152.15 g/eq |
| Ring double bond | 1, conjugated with the anhydride ring |
| PubChem CID | 12475 |
| InChIKey | HMMBJOWWRLZEMI-UHFFFAOYSA-N |
| SMILES | C1CCC2=C(C1)C(=O)OC2=O |
| Appearance | Pale yellow to white flake or solid |
| Melting point | 66 to 69 deg C (up to 72 deg C on the 99% grade) |
| Theoretical iodine value | About 166.8 g I2/100 g |
How This Isomer Fits the Family
Three commercial anhydrides share this chemistry closely enough to be confused, and the differences are worth putting in one table because they decide both the plant and the purchase order.
| Product | CAS | Formula / MW | Melting or crystallisation point | Ring double bond |
|---|---|---|---|---|
| 1,2,3,6-THPA | 85-43-8 | C8H8O3 / 152.15 | About 100 deg C | One, isolated |
| 3,4,5,6-THPA (this product) | 2426-02-0 | C8H8O3 / 152.15 | 66 to 69 deg C | One, conjugated |
| HHPA | 85-42-7 | C8H10O3 / 154.16 | Crystallisation 34 to 38 deg C | None (hydrogenated) |
The isomer pair is the interesting one for a buyer, because two materials with the same formula, the same molecular weight and the same equivalent weight behave differently in the plant: one is a flake that needs a melt tank at 120 to 130 deg C, the other softens below 70 deg C and can be melted in warm water-jacketed equipment. There is no way to tell them apart by assay. The InChIKey and the melting range are the two identifiers that actually separate them.
Manufacture and the Isomer Ratio
The tetrahydrophthalic anhydrides come out of the same Diels-Alder chemistry: butadiene and maleic anhydride combine to build the cyclohexene ring with the anhydride fused to it. The main adduct is the 1,2,3,6-isomer, with the double bond isolated in the ring. The 3,4,5,6-isomer, in which the double bond sits against the anhydride ring, is produced either as a secondary product of that chemistry or deliberately by isomerisation of the main adduct under controlled thermal conditions.
For a buyer the consequence is that the two isomers can be present in each other’s lots, and the melting range is the first sign. A 3,4,5,6-THPA lot melting above 72 deg C is carrying high-melting isomer or diacid; a 1,2,3,6-THPA lot melting below 98 deg C is carrying low-melting isomer. Neither is necessarily a reject, but both change the melt handling and the cure schedule, and both should be explained by the supplier rather than discovered by the customer.
What the Three Grades Are For
| Item | Grade 1 | Grade 2 | Grade 3 (custom) |
|---|---|---|---|
| Appearance | Pale yellow flake | White or off-white solid | White solid |
| Assay | >=96% | >=99% | >=99.5% or >=99.8% |
| Melting point | 66 to 69 deg C | 66 to 72 deg C | On request |
| Typical application | Polyester, alkyd and plasticiser intermediate | General curing and intermediate | Electrical, optical, fine-chemical |
The 96% grade is a feedstock grade
Three to four percent of a 96% lot is the corresponding diacid and low oligomers, and the colour it carries is the pale yellow. For polyester, alkyd and plasticiser routes that is not a defect: the diacid is a reactive participant in those processes, and nobody is measuring the colour of the intermediate. Buying the 99% grade for a resin feedstock is paying for a purity that the process destroys in the first hour.
The 99% grade is the curing grade
White to off-white, with a melting range of 66 to 72 deg C, this is the grade that goes into an epoxy casting or a coating. The slightly wider melting range compared with the 96% grade is normal for a purified product; what matters is that the top of the range stays below the temperature at which the material would start to sit as a slush in the melt line.
The custom grades are for dielectric and optical work
99.5% and 99.8% are ordered where the anhydride is the purity-limiting component of the system, typically electrical insulation with tight dielectric requirements, transparent castings, and applications where the anhydride is a fine-chemical intermediate rather than a bulk hardener.
The Physical Cost of a Low Melting Point
A melting point of 67 deg C is an advantage in the plant and a complication in logistics. Both halves deserve attention.
What the plant gains
- A lower melt temperature. A tank at 80 to 90 deg C rather than 120 to 130 deg C, which cuts heat-up time and reduces the thermal exposure that darkens an anhydride.
- Shorter hold-up. Lower temperature and a shorter melt cycle mean less time at temperature, and less time at temperature means less free acid and less colour drift.
- Blend flexibility. A low-melting isomer can be melted first and used to dissolve a higher-melting component, which is the basis of the eutectic blends used to tune working viscosity.
- Lower viscosity at dosing temperature in many blends, which helps degassing and impregnation of fine windings.
What logistics loses
A product that softens at 67 deg C will soften inside a container standing in a summer yard. Container interiors routinely exceed 60 deg C in direct sun in hot climates, and a pallet of bags near the door can reach the softening range. The material does not decompose, but it fuses into a block, the bags deform, and the customer receives a product that has to be re-melted and re-bagged before it can be dosed.
| Situation | What happens | Practical control |
|---|---|---|
| Temperate climate, short transit | Material arrives as flake | Standard bag with PE liner is adequate |
| Hot climate, container in sun | Fused block, deformed bags | Ventilated or insulated container, pallets away from the door, plan for re-melting |
| Long dwell in a hot warehouse | Partial melting and re-solidification, moisture pick-up at the seams | Temperature-controlled store, sealed liner, first-in first-out |
Anhydride Curing With the Low-Melting Isomer
The dose arithmetic is identical to the other isomer because the equivalent weight is identical:
phr = (AEW / EEW) x 100 x r, with AEW = 152.15 and r = 0.85 to 1.0
| Resin EEW | r = 0.85 | r = 0.90 | r = 1.00 |
|---|---|---|---|
| 185 (standard DGEBA) | 69.9 phr | 74.0 phr | 82.2 phr |
| 200 | 64.7 phr | 68.5 phr | 76.1 phr |
| 250 | 51.7 phr | 54.8 phr | 60.9 phr |
The difference is in the processing window rather than the chemistry. With a lower melting point, the anhydride dissolves into the resin faster at a given temperature, so the vacuum casting cycle can start sooner. That is a real productivity gain in a plant that casts large parts, and it is the main reason a formulator will choose this isomer over the higher-melting one even though the two are chemically equivalent in dose.
Note the reactivity difference that comes with the structure. The double bond in this isomer is conjugated with the anhydride ring, which changes its behaviour in Diels-Alder additions and in radical copolymerisation compared with the isolated double bond of 1,2,3,6-THPA. In an epoxy cure this is a second-order effect, but in a polyester or a grafting reaction it is not, and it is the reason the two isomers are not interchangeable in those systems either.
Applications
- Low-temperature epoxy casting. Shops with existing melt equipment sized for 80 to 90 deg C, and shops that want to avoid running a 130 deg C tank.
- Eutectic anhydride blends. Mixed with a higher-melting anhydride or with MTHPA to reach a melting range and viscosity that suit a particular metering machine.
- Unsaturated polyester and alkyd resins. Usually the 96% grade, where colour is not critical and the double bond participates in the styrene copolymerisation.
- Plasticiser and ester intermediates by ring opening with alcohols.
- Fine-chemical building block where the conjugated double bond is used for cycloaddition or functionalisation.
Storage and Safety
Treat this product as a moisture-sensitive sensitiser with a low softening point. Store sealed, dry and cool, away from steam lines, hot walls and sun-exposed containers, and keep the store below the point at which the flake starts to fuse.
The material hydrolyses to the diacid and becomes corrosive; it is a skin sensitiser and its dust is irritating. Use local exhaust ventilation, gloves, eye protection and a dust mask, clean spills dry, and never wash an anhydride spill down a drain. Keep it away from amines, alkalis, alcohols and accelerators, which react exothermically with anhydrides.
Because the melting point is low, molten handling is easier than for the high-melting isomer and therefore more tempting. A melt tank at 80 deg C still needs a dry, covered system: water in a warm anhydride hydrolyses it faster than water in a cold solid, because the reaction is intimate rather than surface-only.
Buying Checklist
- Confirm the CAS number and the isomer. "Tetrahydrophthalic anhydride" alone is ambiguous; 2426-02-0 is this product and 85-43-8 is the other one.
- Do not confuse TMMA with MTHPA. MTHPA is methyltetrahydrophthalic anhydride, a liquid with a methyl group on the ring; it is a different product with a different CAS number and a different dose.
- Ask for the melting range. It is the cheapest check on purity and isomer content, and it is the one test that catches a mislabelled lot.
- Specify the packing for the climate. For hot destinations, ask for a ventilated container and a moisture-barrier liner rather than a standard bag.
- Match the grade to the use. 96% for resin feedstock, 99% for curing, 99.5% and above for dielectric or optical work.
FAQ
Why is this isomer cheaper than 1,2,3,6-THPA in some markets?
Because it can be produced at a lower purification cost in some process configurations, and because the 96% feedstock grade has a different specification entirely. Compare grades, not just products: a 96% lot and a 99.5% lot are not competing offers, even though they share a CAS number in casual conversation.
Can the two tetrahydrophthalic anhydrides be blended?
Yes, and blending is common practice to tune the melting range. The blend is chemically sensible because the equivalent weights are identical, so the dose does not change; what changes is the melt point of the mix and the crystalline behaviour on cooling.
Is the double bond a problem in an epoxy cure?
Not in the cure itself. The anhydride ring is what reacts with the epoxy. The double bond matters afterwards, in colour stability and in any later reaction that involves unsaturation, which is why colour-critical applications move to HHPA instead.
What purity do I need for a transparent casting?
The 99.5% custom grade at minimum, and 99.8% where the part is optically inspected. Residual diacid and oligomer scatter light and tint the part, and no post-cure removes either effect.
How should I check a delivery?
Melting range on a sample, free acid by titration, colour against a standard, and a visual check for fused blocks and damaged bags. If the melting range is out, stop and ask for the InChIKey before using the lot.
Related Reading
- 3,4,5,6-Tetrahydrophthalic anhydride (TMMA), CAS 2426-02-0 – product page with the three grades.
- THPA: properties, grades and curing – the high-melting isomer in detail.
- THPA vs 3,4,5,6-THPA vs HHPA – the three-product decision table.
- Anhydride dosage in phr – the calculation, the accelerators and the common errors.
- Free acid, colour and moisture control – why these three numbers travel together.
- MTHPA: the liquid member of the family – an extra methyl group, a different formula and a dose about 15% higher.
Disclaimer: this article describes commercial specifications and industrial chemistry. Formulations, cure schedules and regulatory classifications must be validated by the user for the specific application and jurisdiction.
Contact PolyblueChem for a current certificate of analysis, a sample of the 99% or custom grade, and a quotation for bagged or jumbo bag supply.